Degradation/ Oxidation Susceptibility of Composite Semiconductor;Organic Photovoltaic cell of ZnO/PEDOT: PSS/Graphite
DOI:
https://doi.org/10.24218/jnat.2017.29Keywords:
Degradation/Oxidation, Organic Photovoltaic (OPV) Cells, Power Conversion Efficiency (PCE), Electrochemical Impedance Spectroscopy (EIS), Aqueous SolutionsAbstract
A criterion of the degradation/oxidation susceptibility of organic photovoltaic (OPV) cells free of any metallic electrodes is considered. This criterion is used to determine the degradation/ oxidation of ZnO/PEDOT: PSS/Graphite cells in deionized water and in also polluted water with fine particles of sand. The values of Rp s were determined by the electrochemical impedance spectroscopy (EIS) at a low frequency. In addition, results of the criterion of ZnO/PEDOT: PSS/Graphite cells was compared with ZnO/PEDOT: PSS/Silver cells in similar media for a predetermined period of OPV operations. In the meantime, the ZnO/PEDOT: PSS/Graphite cell was found to have good degradation resistance during 1000 hrs of exposure to deionized water and polluted water with respect to the standard plots of lim (Rp s./Rpair) versus time of exposure.Downloads
Published
2018-11-22
Issue
Section
Research